The main products are contents:mullite light-weight brick£¬high-temperature bonder and indeterminate from fireproofing material etc.
classification
Application:
Wall and lining thermal insulation material of various thermal treatment furnace carburizing furnace, nitriding furnace and other industrial furnaces.
Feature£º
Extrusion molding is used, anti-permeability carbon, high-aluminum low-iron brick produced by secondary processing craft, which is of low iron content, high anti-carburi-zation, low coefficient of heat conductivity and uniform internal structure
Physical and chemical indicators
Physical and chemical indicators£º
Name of commodity Performance and index |
Anti carburizing bricks | High aluninum low iron brick | ||||||
KST0.6 | KST0.8 | KST1.0 | KST2.0 | KST2.5 | ZDLG0.6 | ZDLG0.8 | ||
Bulk density g£¯cm | 0.6 | 0.8 | 1 | 2 | 2.5 | 0.6 | 0.8 | |
Compressive strength Mpa | 2 | 3 | 4 | 25 | 35 | 2 | 3.5 | |
Linear change on reheating ¡æXhr£¥¡Ü | 1250*12 0.5 | 1300*12 0.4 | 1300*12 0.4 | 1300*12 0.2 | 1300*12 0.2 | 1400*4 0.5 | 1400*4 0.5 | |
A12O3 £¥ ¡Ý | 42 | 46 | 48 | 50 | 56 | 50 | 52 | |
SiO2 £¥ ¡Ü | 56 | 52 | 50 | 48 | 42 | 48 | 46 | |
Fe2O3 £¥ ¡Ü | 0.7 | 0.7 | 0.7 | 0.7 | 0.7 | 0.5 | 0.5 | |
Heat conductivity ¡Ü350¡À20¡æw£¯m.k | 0.25 | 0.35 | 0.45 | 1.6 | ¡¡ | 0.25 | 0.3 | |
Highest use temp ¡æ | 1250 | 1300 | 1350 | 1350 | 1350 | 1350 | 1350 | |
Load softening temp ¡æ | 1280 | 1350 | 1400 | 1400 | 1400 | 1400 | 1400 |
The actual parameters can be adjusted according to the requirements of users.